Ferrite C5 has a remanence Br of 3.8 kG (0.38 T), an intrinsic coercivity HcJ of at least 2.5 kOe (199 kA/m) and a maximum energy product of 3.4 MGOe (27 kJ/m³). Typical maximum working temperature: 250°C (482°F).
- BrRemanence
- 0.38 T3.8 kG3.8 kG0.38 T
- (BH)maxMax. energy product
- 27 kJ/m³3.4 MGOe3.4 MGOe27 kJ/m³
- HcJIntrinsic coercivity (min.)
- 199 kA/m2.5 kOe2.5 kOe199 kA/m
- TmaxMax. working temp. (typical)
- 250°C482°F482°F250°C
Drawing
Ferrite C5 specifications
| BrRemanence | 3.8 kG0.38 T |
|---|---|
| HcJIntrinsic coercivity (min.) | 2.5 kOe199 kA/m |
| (BH)maxMax. energy product | 3.4 MGOe27 kJ/m³ |
| TmaxMax. working temp. (typical) | 250°C482°F |
| Material | Hard ferrite (SrFe/BaFe) |
Ferrite C5 (ceramic 5) is the standard anisotropic ferrite for loudspeakers, motors and holding magnets. Values are MMPA nominal figures; Chinese grade Y30 is similar.
Also known as
C5Y30
All magnet grades
Sources
- IEC 60404-8-1:2015, Magnetic materials, Part 8-1: Specifications for individual materials, Magnetically hard materials
- GB/T 13560-2017: Sintered neodymium iron boron permanent magnets (grade structure)
- MMPA Standard 0100-00: Standard specifications for permanent magnet materials (ferrite C5, C8)
- Arnold Magnetic Technologies: Neodymium and ferrite magnet grade data sheets