N42SH Magnet Grade Properties
Magnet Grades · SH: HcJ ≥ 20 kOe, 150 °C
N42SH has a remanence Br of 12.8–13.2 kG (1.28–1.32 T), an intrinsic coercivity HcJ of at least 20 kOe (1592 kA/m) and a maximum energy product of 40–43 MGOe (318–342 kJ/m³). Typical maximum working temperature: 150°C (302°F).
- BrRemanence
- 1.28–1.32 T12.8–13.2 kG12.8–13.2 kG1.28–1.32 T
- (BH)maxMax. energy product
- 318–342 kJ/m³40–43 MGOe40–43 MGOe318–342 kJ/m³
- HcJIntrinsic coercivity (min.)
- 1592 kA/m20 kOe20 kOe1592 kA/m
- TmaxMax. working temp. (typical)
- 150°C302°F302°F150°C
Drawing
N42SH specifications
| BrRemanence | 12.8–13.2 kG1.28–1.32 T |
|---|---|
| HcJIntrinsic coercivity (min.) | 20 kOe1592 kA/m |
| (BH)maxMax. energy product | 40–43 MGOe318–342 kJ/m³ |
| TmaxMax. working temp. (typical) | 150°C302°F |
| Material | Sintered NdFeB |
N42SH is a frequent choice for motors and generators: Br close to N42 with HcJ ≥ 20 kOe for operation to about 150 °C.
Also known as
42SH
Same energy product in other coercivity classes
Other grades in this class
All magnet grades
Sources
- IEC 60404-8-1:2015, Magnetic materials, Part 8-1: Specifications for individual materials, Magnetically hard materials
- GB/T 13560-2017: Sintered neodymium iron boron permanent magnets (grade structure)
- MMPA Standard 0100-00: Standard specifications for permanent magnet materials (ferrite C5, C8)
- Arnold Magnetic Technologies: Neodymium and ferrite magnet grade data sheets
Values last checked against these sources on November 15, 2026. · How we check data
Reference values for planning and identification. Confirm critical dimensions with the manufacturer's drawing or the current edition of the standard before production.