Magnet Grades · N: standard (HcJ ≥ 11–12 kOe, 80 °C)

N42 has a remanence Br of 12.8–13.2 kG (1.28–1.32 T), an intrinsic coercivity HcJ of at least 12 kOe (955 kA/m) and a maximum energy product of 40–43 MGOe (318–342 kJ/m³). Typical maximum working temperature: 80°C (176°F).

BrRemanence
1.28–1.32 T12.8–13.2 kG12.8–13.2 kG1.28–1.32 T
(BH)maxMax. energy product
318–342 kJ/m³40–43 MGOe40–43 MGOe318–342 kJ/m³
HcJIntrinsic coercivity (min.)
955 kA/m12 kOe12 kOe955 kA/m
TmaxMax. working temp. (typical)
80°C176°F176°F80°C

Drawing

0−250−500−750−1000−12500.00.20.40.60.81.01.21.41.6Field strength H, kA/m (reverse)B, J (T)Br 1.28 TBr 12.8 kGHcJ 955 kA/mHcJ 12 kOeB (normal)J (intrinsic)
Idealized room-temperature demagnetization curves from the minimum Br and HcJ of the grade; use the producer's data sheet for design.Proportions shown, not to scale

N42 specifications

BrRemanence12.8–13.2 kG1.28–1.32 T
HcJIntrinsic coercivity (min.)12 kOe955 kA/m
(BH)maxMax. energy product40–43 MGOe318–342 kJ/m³
TmaxMax. working temp. (typical)80°C176°F
MaterialSintered NdFeB

N42 is the most common general-purpose grade: a good balance of strength and price.

Also known as

42

Same energy product in other coercivity classes

Other grades in this class

All magnet grades

Compare all 39 grades in the Magnet Grades chart →

Sources

  1. IEC 60404-8-1:2015, Magnetic materials, Part 8-1: Specifications for individual materials, Magnetically hard materials
  2. GB/T 13560-2017: Sintered neodymium iron boron permanent magnets (grade structure)
  3. MMPA Standard 0100-00: Standard specifications for permanent magnet materials (ferrite C5, C8)
  4. Arnold Magnetic Technologies: Neodymium and ferrite magnet grade data sheets

Values last checked against these sources on November 15, 2026. · How we check data