N50 Magnet Grade Properties
Magnet Grades · N: standard (HcJ ≥ 11–12 kOe, 80 °C)
N50 has a remanence Br of 14–14.5 kG (1.40–1.45 T), an intrinsic coercivity HcJ of at least 11 kOe (875 kA/m) and a maximum energy product of 48–51 MGOe (382–406 kJ/m³). Typical maximum working temperature: 80°C (176°F).
- BrRemanence
- 1.40–1.45 T14–14.5 kG14–14.5 kG1.40–1.45 T
- (BH)maxMax. energy product
- 382–406 kJ/m³48–51 MGOe48–51 MGOe382–406 kJ/m³
- HcJIntrinsic coercivity (min.)
- 875 kA/m11 kOe11 kOe875 kA/m
- TmaxMax. working temp. (typical)
- 80°C176°F176°F80°C
Drawing
N50 specifications
| BrRemanence | 14–14.5 kG1.40–1.45 T |
|---|---|
| HcJIntrinsic coercivity (min.) | 11 kOe875 kA/m |
| (BH)maxMax. energy product | 48–51 MGOe382–406 kJ/m³ |
| TmaxMax. working temp. (typical) | 80°C176°F |
| Material | Sintered NdFeB |
Also known as
50
Same energy product in other coercivity classes
Other grades in this class
All magnet grades
Sources
- IEC 60404-8-1:2015, Magnetic materials, Part 8-1: Specifications for individual materials, Magnetically hard materials
- GB/T 13560-2017: Sintered neodymium iron boron permanent magnets (grade structure)
- MMPA Standard 0100-00: Standard specifications for permanent magnet materials (ferrite C5, C8)
- Arnold Magnetic Technologies: Neodymium and ferrite magnet grade data sheets
Values last checked against these sources on November 15, 2026. · How we check data